Description: Leadless high alkali borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 17.70% | 0.50 | |
| Na2O | 11.65% | 0.50 | |
| B2O3 | 26.16% | 1.00 | |
| Al2O3 | 3.83% | 0.10 | |
| SiO2 | 40.66% | 1.80 | |
| Oxide Weight | 266.10 | ||
| Formula Weight | 266.10 | ||
| Materials |
Frit 6004
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |