Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 4712

Alternate Names: Frit 4712

Description: Borosilicate hard clear general purpose frit 1040-1100C

Oxide Analysis Formula Tolerance
CaO 9.55% 0.60
K2O 3.47% 0.13
Na2O 4.75% 0.27
B2O3 12.44% 0.63
Al2O3 10.13% 0.35
SiO2 59.67% 3.50
Oxide Weight 352.54
Formula Weight 352.54

Notes

General purpose and versatile frit, good for strong and underglaze colors.
New name is Frit 4113.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 4113
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved