Alternate Names: F3211
Description: Calcium Borate Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 42.00% | 1.00 | |
| B2O3 | 58.00% | 1.11 | |
| Oxide Weight | 133.57 | ||
| Formula Weight | 133.57 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Keramikos Fritte 32.21
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.5 |
|---|---|
| Frit Melting Range (C) | 1750F |