Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 6.00% | 0.28 | |
| K2O | 9.00% | 0.25 | |
| Na2O | 11.00% | 0.47 | |
| Al2O3 | 9.00% | 0.23 | |
| B2O3 | 15.00% | 0.57 | |
| SiO2 | 50.00% | 2.19 | |
| Oxide Weight | 263.22 | ||
| Formula Weight | 263.22 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |