Description: Medium zinc opacified frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZnO | 6.56% | 0.20 | |
| MgO | 3.28% | 0.21 | |
| ZrO2 | 7.89% | 0.16 | |
| Al2O3 | 7.11% | 0.18 | |
| Fe2O3 | 0.14% | - | |
| K2O | 4.08% | 0.11 | |
| TiO2 | 0.08% | - | |
| Na2O | 0.49% | 0.02 | |
| SiO2 | 58.56% | 2.46 | |
| CaO | 10.23% | 0.46 | |
| LOI | 1.49% | n/a | |
| Oxide Weight | 248.82 | ||
| Formula Weight | 252.58 | ||
| Typecodes |
Frit