| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.39% | 0.03 | |
| K2O | 1.16% | 0.05 | |
| MgO | 0.07% | 0.01 | |
| Na2O | 1.16% | 0.07 | |
| TiO2 | 1.97% | 0.09 | |
| Al2O3 | 27.66% | 1.00 | |
| SiO2 | 54.25% | 3.33 | |
| Fe2O3 | 1.50% | 0.03 | |
| LOI | 11.84% | n/a | |
| Oxide Weight | 325.10 | ||
| Formula Weight | 368.76 | ||
| Materials |
Fireclay
|
| Typecodes |
Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service. |
| Typecodes |
Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more. |