Oxide Analysis Formula Tolerance
SiO2 48.30% 2.23
Al2O3 36.70% 1.00
K2O 4.25% 0.13
Fe2O3 0.69% 0.01
MgO 0.12% 0.01
Na2O 0.21% 0.01
TiO2 0.35% 0.01
LOI 8.00%n/a
Oxide Weight 251.86
Formula Weight 273.76

Notes

CD-3200 is a water ground muscovite mica that has optimum delamination and high purity. Our patented process produces a mica product that gives optimum performance in a variety of applications. In addition to excellent color, CD-3200 creates a functional pigment that is very desirable where low bulk density, fineness, high aspect ratio, and excellent coverage are required.

Performance Characteristics

The performance characteristics that make
CD-3200 an acceptable cost effective additive for these markets are:
Excellent color
Ease of dispersion
Increased coverage
Chemical inertness
Superior barrier properties
High temperature stability
Superior dielectric properties
Superior reinforcement properties

Mean Particle Size, microns 15 - 25 18
Sieve Analysis, % retained
+100 mesh Trace Trace
+200 mesh 1.0 max. 0.8
+325 mesh 4 - 12 6
Bulk Density (Colgate method) 8 - 14 12
Moisture Loss, 100Cº, % <0.5
Color, L value >90

Mineral Muscovite mica
Chemical Composition Potassium aluminum silicate
Specific gravity 2.82
CAS# 12001-26-2
ph 6.0 - 7.5

Related Information

Links

URLs http://www.gimmica.com/
Company website
Materials Mica
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy