Description: Cuban kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 52.10% | 2.81 | |
| Al2O3 | 31.50% | 1.00 | |
| Fe2O3 | 1.70% | 0.03 | |
| TiO2 | 1.00% | 0.04 | |
| CaO | 0.55% | 0.03 | |
| MgO | 0.46% | 0.04 | |
| K2O | 1.90% | 0.07 | |
| Na2O | 0.09% | - | |
| LOI | 10.30% | n/a | |
| Oxide Weight | 289.16 | ||
| Formula Weight | 322.37 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Materials |
Arcilla de Pontezuelo (Cuba)
|
| Materials |
Caolín Blanco (Cuba)
|
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk