BPS Cornish Stone

Oxide Analysis Formula Tolerance
CaO 1.49% 0.19
K2O 4.52% 0.35
MgO 0.14% 0.02
Na2O 3.48% 0.41
TiO2 0.06% 0.01
Al2O3 15.49% 1.11
P2O5 0.48% 0.02
SiO2 74.22% 8.99
Fe2O3 0.13% 0.01
Oxide Weight 728.33
Formula Weight 728.33

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
Materials Cornwall Stone

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy