Alternate Names: Iron(II) Sulphate, Iron(II) Sulfate
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Fe2O3 | 57.50% | 1.00 | |
| LOI | 42.50% | n/a | |
| Oxide Weight | 160.00 | ||
| Formula Weight | 278.26 | ||
| Materials |
Spanish Red Iron Oxide
|
| Materials |
Iron Oxide Red
Red iron oxide is the most common colorant used in ceramic bodies and glazes. As a powder, it is available in red, yellow, black and other colors. |
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |