Fusion Frit F-71

Alternate Names: Fusion Frit F71

Description: Alkaline flux for grinding wheels

Oxide Analysis Formula Tolerance
CaO 6.00% 0.23
K2O 2.50% 0.06
Na2O 20.40% 0.71
B2O3 6.00% 0.19
Al2O3 6.80% 0.14
SiO2 58.30% 2.10
Oxide Weight 216.21
Formula Weight 216.21

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3281
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 11.31 x 10-6
Frit Softening Point 1400F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy