James Kent Frit DR1327

Description: Zinc barium calcium alkali frit (formerly #FT0540)

Oxide Analysis Formula Tolerance
BaO 3.00% 0.06
CaO 11.00% 0.58
KNaO 9.00% 0.34
ZnO 10.00% 0.36
B2O3 6.00% 0.25
Al2O3 8.00% 0.23
SiO2 56.00% 2.75
Oxide Weight 304.29
Formula Weight 304.29

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 0.335 @ 500C