Description: LEADLESS FRIT
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 2.56% | 0.07 | |
| CaO | 7.89% | 0.61 | |
| K2O | 3.75% | 0.17 | |
| MgO | 0.49% | 0.05 | |
| Na2O | 1.12% | 0.08 | |
| SrO | 0.27% | 0.01 | |
| B2O3 | 16.88% | 1.05 | |
| Al2O3 | 10.92% | 0.47 | |
| SiO2 | 56.12% | 4.06 | |
| Oxide Weight | 434.82 | ||
| Formula Weight | 434.82 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |