Description: Strontium calcium silicate frit
Oxide | Analysis | Formula | Tolerance |
---|---|---|---|
CaO | 9.73% | 0.53 | |
K2O | 2.96% | 0.10 | |
Li2O | 0.41% | 0.04 | |
MgO | 0.72% | 0.06 | |
Na2O | 2.79% | 0.14 | |
SrO | 4.43% | 0.13 | |
B2O3 | 5.26% | 0.23 | |
Al2O3 | 12.12% | 0.37 | |
SiO2 | 61.58% | 3.16 | |
Oxide Weight | 308.41 | ||
Formula Weight | 308.41 |
Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
Materials |
Ferro Frit 3292
|
Materials |
Fusion Frit F-134
|
Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
Co-efficient of Linear Expansion | 7.30 |
---|---|
Frit Softening Point | 1750F |