Ferro Frit 3626

Description: Lead bisilicate frit

Oxide Analysis Formula Tolerance
PbO 65.00% 1.00
SiO2 35.00% 2.00
Oxide Weight 343.38
Formula Weight 343.38

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials BPS Lead Bisilicate
Materials Ceraflux
An alumina lead bisilicate from Hammond Lead Products in Indiana. The data sheet claims it is safe and insoluble in stomach acid.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 820C M
Density (Specific Gravity) 4.50

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy