Ferro Frit 3497

Description: Medium lead zincless frit cone 2-5

Oxide Analysis Formula Tolerance
CaO 9.50% 0.55
K2O 1.50% 0.05
Na2O 2.50% 0.13
PbO 19.00% 0.27
B2O3 5.00% 0.23
Al2O3 5.50% 0.17
SiO2 57.00% 3.05
Oxide Weight 321.84
Formula Weight 321.84

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit L-294-J
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.20