Ferro Frit 3476

Description: High lead borosilicate frit

Oxide Analysis Formula Tolerance
PbO 63.30% 1.00
B2O3 19.80% 1.00
SiO2 16.90% 0.99
Oxide Weight 352.61
Formula Weight 352.61

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 4GF63D
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.0
Frit Melting Range (C) 1050F
By Tony Hansen