Ferro Frit 3211

Alternate Names: F3211

Description: Calcium Borate Frit

Oxide Analysis Formula Tolerance
CaO 42.00% 1.00
B2O3 58.00% 1.11
Oxide Weight 133.57
Formula Weight 133.57

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Keramikos Fritte 32.21
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.5
Frit Melting Range (C) 1750F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy