| Monthly Tech-Tip | No tracking! No ads! |
Alternate Names: F3191
Description: A source of alkali borate for use in abrasives industry
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 11.27% | 0.50 | |
| Na2O | 12.46% | 0.50 | |
| B2O3 | 27.97% | 1.00 | |
| SiO2 | 48.30% | 2.00 | |
| Oxide Weight | 248.84 | ||
| Formula Weight | 248.84 | ||
| Materials |
Fusion Frit F-34
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 9.2 x 10-6 (50-450C) |
|---|---|
| Frit Melting Range (C) | 1300F |
| By Tony Hansen Follow me on ![]() | ![]() |