G2926B Base

Description: Cone 6 glossy base glaze

Oxide Analysis Formula Tolerance
CaO 5.00% 0.48
K2O 0.88% 0.05
MgO 0.72% 0.10
Na2O 4.26% 0.37
B2O3 5.63% 0.44
Al2O3 11.74% 0.62
SiO2 68.62% 6.17
LOI 3.00%n/a
Oxide Weight 523.39
Formula Weight 539.58

Notes

Clear base sold as a powder by Plainsman Clays. The recipe and usage of G2926B are well documented online.