1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Mondre and Manz Frit V15098

Description: Zinc alkali frit

Oxide Analysis Formula Tolerance
K2O 10.60% 0.35
CaO 5.05% 0.28
Al2O3 11.48% 0.35
Li2O 0.86% 0.09
ZnO 7.33% 0.28
B2O3 3.58% 0.16
SiO2 61.09% 3.16
Oxide Weight 311.06
Formula Weight 311.06

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy