Colorobbia Frit 250

Description: High zinc opacified frit

Oxide Analysis Formula Tolerance
ZnO 11.43% 0.34
Al2O3 6.99% 0.17
ZrO2 9.78% 0.19
MgO 2.35% 0.14
Na2O 0.56% 0.02
SiO2 55.40% 2.24
K2O 4.02% 0.10
Fe2O3 0.13% -
CaO 9.05% 0.39
TiO2 0.08% -
LOI 0.11%n/a
Oxide Weight 242.35
Formula Weight 242.62

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy