Glasurfritten 37.025

Alternate Names: 37 025,37-025

Description: Bleifreie Alkali-Bor-Fritte

Oxide Analysis Formula Tolerance
Na2O 15.00% 1.00
B2O3 34.00% 2.02
SiO2 51.00% 3.51
Oxide Weight 413.33
Formula Weight 413.33

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 82 x 10-7
Frit Softening Point 548C
Frit Melting Range (C) 900-1100C