Alternate Names: 35 32,35-32
Description: Blei-Bor-Silikat-Fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 68.57% | 1.00 | |
| B2O3 | 19.80% | 0.93 | |
| SiO2 | 11.63% | 0.63 | |
| Oxide Weight | 325.51 | ||
| Formula Weight | 325.51 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 75 x 10-7 |
|---|---|
| Frit Softening Point | 473C |
| Frit Melting Range (C) | 800-1080C |