Frit VO 6253

Description: Reimbold & Strick stoneware frit

Oxide Analysis Formula Tolerance
K2O 3.00% 0.07
BaO 10.00% 0.15
ZnO 4.00% 0.11
CaO 13.00% 0.52
Li2O 2.00% 0.15
Al2O3 5.00% 0.11
B2O3 6.00% 0.19
SiO2 57.00% 2.13
Oxide Weight 224.69
Formula Weight 224.69

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 67 x 10-7 (20-400C)
Frit Softening Point 620C
Glass Transition Temperature 570C