Frit A 3368

Description: Reimbold & Strick manganese frit

Oxide Analysis Formula Tolerance
B2O3 13.00% 0.75
CaO 3.00% 0.22
Na2O 5.00% 0.32
BaO 10.00% 0.26
SiO2 45.00% 3.01
ZnO 4.00% 0.20
Al2O3 5.00% 0.20
Oxide Weight 342.06
Formula Weight 342.06

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 59 x 10-7 (20-400C)
Frit Softening Point 510C
Glass Transition Temperature 480C