Zircosil

Description: Zircopax Plus made by Endeka Ceramics

Notes

This is available in many particle sizes, each used for a specific industry or family of applications. Examples grade grades are S, D, 200, 200M, 300M, Ten, Five, One (the latter referring to micron sizes). The Five material is sold as "Zircopax Plus" in North America.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Zircopax
Zirconium silicate, its principle use in ceramics is as an opacifier in glazes. It is an expensive material, but less so than tin oxide.
Materials Zircopax Plus

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy