Digitalfire is facing a takedown order from Plainsman Clays. They are revoking permission to "use any Plainsman content" "on any platform". This is broad and vague enough, and this site large enough, that I am unable to comply or even interpret it in the short timeframe (June 27). Insight-live.com general operation is not affected by this.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

FM Fireclay

Oxide Analysis Formula Tolerance
CaO 0.16% 0.01
K2O 1.88% 0.09
MgO 0.69% 0.08
Na2O 0.04% -
TiO2 1.32% 0.08
Al2O3 21.96% 1.00
P2O5 0.06% -
SiO2 64.63% 4.99
Fe2O3 1.29% 0.04
LOI 7.97%n/a
Oxide Weight 427.46
Formula Weight 464.48

Related Information

Links

Materials Fireclay
Typecodes Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service.
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy