Ferro Frit CC-263-2

Description: GLAZE FRIT CONE 04-2

Oxide Analysis Formula Tolerance
CaO 7.50% 0.65 2.5
K2O 2.50% 0.13 2.5
MgO 0.50% 0.06 .5
Na2O 0.50% 0.04 .5
SrO 2.50% 0.12 2.5
ZrO2 0.50% 0.02 .5
B2O3 17.50% 1.23 2.5
Al2O3 12.50% 0.60 2.5
SiO2 52.50% 4.26 2.5
Oxide Weight 471.12
Formula Weight 471.12

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit CC-263
Materials Ferro Frit CC-272
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Available from Laguna Clays

Data

Co-efficient of Linear Expansion 6.79 x 10-6
Frit Softening Point 1850F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy