Oxide Analysis Formula Tolerance
Na2O 6.00% 0.33
CaO 11.00% 0.67
B2O3 22.50% 1.10
Al2O3 12.00% 0.40
SiO2 48.50% 2.76
Oxide Weight 341.47
Formula Weight 341.47

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Ferro Frit 3195
A commonly available calcium borosilicate frit. It is glaze-like, needing only a kaolin addition to create a low-temperature semi-glossy glaze.

Data

Co-efficient of Linear Expansion 71.6 (10-7/C 20/300C)
Frit Melting Range (C) 1000-1300C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy