1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Feldspar HolguĂ­n (Cuba)

Description: Cuban feldspar

Oxide Analysis Formula Tolerance
SiO2 71.90% 8.13
Al2O3 17.18% 1.14
TiO2 0.01% -
CaO 2.20% 0.27
MgO 0.48% 0.08
K2O 1.22% 0.09
Na2O 5.15% 0.56
Fe2O3 0.31% 0.01
LOI 1.00%n/a
Oxide Weight 669.08
Formula Weight 675.84

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.