Description: Cuban feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 72.00% | 7.36 | |
| Al2O3 | 15.40% | 0.93 | |
| TiO2 | 0.01% | - | |
| CaO | 1.40% | 0.15 | |
| MgO | 0.85% | 0.13 | |
| K2O | 4.30% | 0.28 | |
| Na2O | 4.40% | 0.44 | |
| Fe2O3 | 0.27% | 0.01 | |
| 1.00% | - | ||
| LOI | 1.00% | n/a | |
| Oxide Weight | 606.35 | ||
| Formula Weight | 612.47 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| Materials |
Feldspar HolguĂn (Cuba)
|