PotteryCrafts Frit P2963

Alternate Names: Potterycrafts Frit 2963

Description: Soft alkaline very high expansion frit

Oxide Analysis Formula Tolerance
Al2O3 4.90% 0.10
K2O 0.30% 0.01
CaO 26.50% 0.99
MgO 0.10% 0.01
B2O3 10.80% 0.32
SiO2 52.70% 1.83
LOI 4.70%n/a
Oxide Weight 199.36
Formula Weight 209.19

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information

Data

Co-efficient of Linear Expansion 14.5
Frit Melting Range (C) 850-1000C