Description: Swedish feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 75.60% | 10.31 | |
| Al2O3 | 14.50% | 1.17 | |
| Na2O | 4.80% | 0.63 | |
| K2O | 4.20% | 0.37 | |
| Fe2O3 | 0.14% | 0.01 | |
| LOI | 0.60% | n/a | |
| Oxide Weight | 813.41 | ||
| Formula Weight | 818.32 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| URLs |
http://ceramics.sibelcotools.com/tiles/porcelain-tiles/feldspar/
Sibelco Feldspar data |