White Clay C-WC12

Oxide Analysis Formula Tolerance
CaO 1.14% 0.07
MgO 0.47% 0.04
K2O 1.45% 0.05
Na2O 0.13% 0.01
TiO2 0.01% -
Al2O3 29.20% 1.00
SiO2 56.31% 3.27
Fe2O3 0.01% -
LOI 11.14%n/a
Oxide Weight 309.91
Formula Weight 348.76

Notes

A New Zealand material.

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy