Alternate Names: Fusion Frit FZ 580
Description: Fast fire zinc opaque frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 4.80% | 0.10 | |
| Na2O | 1.60% | 0.05 | |
| CaO | 10.60% | 0.39 | |
| MgO | 3.00% | 0.15 | |
| ZnO | 12.00% | 0.30 | |
| Al2O3 | 6.20% | 0.12 | |
| B2O3 | 2.00% | 0.06 | |
| SiO2 | 49.80% | 1.70 | |
| ZrO2 | 10.00% | 0.17 | |
| Oxide Weight | 205.10 | ||
| Formula Weight | 205.10 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.8 x 10-6 |
|---|---|
| Frit Softening Point | 1800F |