Tungsten Trioxide

Alternate Names: Tungsten(VI) oxide, Tungsten Oxide

Formula: WO3

Oxide Analysis Formula Tolerance
WO3 100.00% 1.00
Oxide Weight 231.84
Formula Weight 231.84

Related Information

Links

Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
Materials Tungsten Sulfide
URLs http://en.wikipedia.org/wiki/Tungsten(VI)_oxide
Tungsten Oxide at Wikipedia