Alternate Names: 90420 Zinkbariumfritte
Description: Zinc barium frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZnO | 19.34% | 0.46 | |
| BaO | 35.00% | 0.44 | |
| Li2O | 1.40% | 0.09 | |
| SiO2 | 41.29% | 1.33 | |
| Na2O | 0.10% | - | |
| K2O | 0.10% | - | |
| Al2O3 | 2.79% | 0.05 | |
| Oxide Weight | 194.04 | ||
| Formula Weight | 194.04 | ||
As of 2014, this frit is available in Europe. In Dec 2014 we corrected the chemistry, it was in error before.
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Materials |
Ferro Frit FB-284-M
|
| Materials |
Mondre and Manz Frit 4067
|
| Materials |
Keramikos Bariumzink Fritte
|
| Co-efficient of Linear Expansion | 105 x 10-7 (20-400C) |
|---|---|
| Heating Microscope Analysis for Frits | 555C |
| Heating Microscope Analysis for Frits | 835C |
| Heating Microscope Analysis for Frits | 990C |