Alternate Names: Mount Pinatubo Volcanic Ash
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 5.60% | 0.39 | |
| MgO | 2.70% | 0.26 | |
| K2O | 1.60% | 0.07 | |
| Na2O | 4.40% | 0.28 | |
| Fe2O3 | 5.60% | 0.14 | |
| TiO2 | 0.80% | 0.04 | |
| Al2O3 | 16.10% | 0.62 | |
| SiO2 | 61.90% | 4.04 | |
| LOI | 1.30% | n/a | |
| Oxide Weight | 387.40 | ||
| Formula Weight | 392.51 | ||
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Materials |
Volcanic Ash
Powdered volcanic ash is used to make ceramic glazes, some varieties have a chemistry similar enough to glaze that high percentages can be employed. |
| Materials |
Mt. St. Helens Ash
|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk