Sodium Fluosilicate

Alternate Names: Sodium Silcofluoride

Formula: Na2SiF6

Oxide Analysis Formula Tolerance
Na2O 44.05% 1.00
F 54.00% 4.00
SiO2 28.47% 0.67
Oxide Weight 178.08
Formula Weight 178.08

Notes

This material has a complex reaction during firing similar to Cryolite. Since it gains weight on firing its analysis totals more than 100.

Related Information

Links

Materials Cryolite
Materials Fluorspar
Oxides F - Fluorine
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy