Earth's Crust

Oxide Analysis Formula Tolerance
BaO 0.03% -
CaO 5.08% 0.33
K2O 3.12% 0.12
MgO 3.46% 0.31
Na2O 3.81% 0.22
PbO 0.00% -
SrO 0.04% -
ZnO 0.02% -
TiO2 0.73% 0.03
ZrO2 0.03% -
Al2O3 15.40% 0.55
P2O5 0.27% 0.01
SiO2 53.50% 3.25
Free SiO2 5.80% -
Cr2O3 0.03% -
CuO 0.01% -
Fe2O3 7.15% 0.16
MnO 0.13% 0.01
Oxide Weight 339.16
Formula Weight 339.16

Notes

An average analysis of the principal ceramic minerals in the earths crust.


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy