Sr Metaborate and Sr Pyroborate Eutectic

Oxide Analysis Formula Tolerance
SrO 67.60% 1.00
B2O3 32.40% 0.71
Oxide Weight 153.25
Formula Weight 153.25

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 980C