| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 6.63% | 0.18 | |
| Na2O | 3.07% | 0.13 | |
| CaO | 6.14% | 0.28 | |
| MgO | 1.59% | 0.10 | |
| ZnO | 10.00% | 0.31 | |
| Al2O3 | 13.27% | 0.33 | |
| B2O3 | 4.75% | 0.17 | |
| SiO2 | 51.58% | 2.19 | |
| ZrO2 | 2.97% | 0.06 | |
| Oxide Weight | 255.33 | ||
| Formula Weight | 255.33 | ||
| Materials |
Fusion Frit FZ-164
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.9 x 10-6 |
|---|---|
| Frit Melting Range (C) | 1600F |