Fusion Frit FZ-565

Alternate Names: Fusion Frit FZ565

Description: CaZn frit for slow fire

Oxide Analysis Formula Tolerance
Al2O3 8.50% 0.17
MgO 0.50% 0.03
ZnO 11.20% 0.28
CaO 13.50% 0.49
Na2O 5.80% 0.19
K2O 0.50% 0.01
B2O3 1.50% 0.04
SiO2 58.50% 1.99
Oxide Weight 204.29
Formula Weight 204.29

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.78 x 10-6
Frit Softening Point 1550F