Alternate Names: Fusion Frit F502
Description: Strontium barium frit for dinnerware
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 2.20% | 0.10 | |
| K2O | 1.00% | 0.03 | |
| CaO | 12.10% | 0.63 | |
| SrO | 8.30% | 0.23 | |
| Al2O3 | 5.80% | 0.17 | |
| B2O3 | 9.50% | 0.40 | |
| SiO2 | 61.10% | 2.97 | |
| Oxide Weight | 292.48 | ||
| Formula Weight | 292.48 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.43 x 10-6 |
|---|---|
| Frit Softening Point | 1800F |