Hydrated Lime

Alternate Names: Slaked Lime, Calcium Hydroxide, Calcium Hydrate

Formula: CaO.H2O or Ca(OH)2

Oxide Analysis Formula Tolerance
CaO 75.71% 1.00
H2O 24.30%n/a
Oxide Weight 56.10
Formula Weight 74.11

Notes

Used as a source of CaO in the glass industry.

Related Information

Links

Materials Lime
URLs http://en.wikipedia.org/wiki/Hydrated_lime
Hydrated lime at Wikipedia
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Temperatures Hydrated lime decomposes (25% H2O) (512-)

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy