Johnson Matthey Frit 169

Alternate Names: Frit NR169, Fritte NR 169, Frit NR 169

Description: Barium frit

Oxide Analysis Formula Tolerance
Na2O 19.20% 0.64
CaO 2.30% 0.09
BaO 9.10% 0.12
ZnO 5.80% 0.15
B2O3 28.40% 0.85
Al2O3 0.30% 0.01
SiO2 34.90% 1.21
Oxide Weight 207.78
Formula Weight 207.78

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Johnson Matthey Frit 623
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 700 C