Description: Originally from Harris Mining Co.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 45.72% | 2.07 | |
| Al2O3 | 37.53% | 1.00 | |
| Fe2O3 | 1.16% | 0.02 | |
| TiO2 | 0.08% | - | |
| K2O | 1.17% | 0.03 | |
| Na2O | 0.15% | 0.01 | |
| LOI | 14.04% | n/a | |
| Oxide Weight | 233.22 | ||
| Formula Weight | 271.31 | ||
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |