Ferro Frit CC-261

Alternate Names: Frit CC261

Description: Zinc frit

Oxide Analysis Formula Tolerance
ZnO 10.90% 1.00
Oxide Weight 81.40
Formula Weight 81.40

Notes

SiO2:Al2O3 ratio is 11.51
Alkalies: 5-15%
CaO 5-15%
MgO less than 5%
Al2O3 5-15%
B2O3 less than 5%
SiO2 over 50%

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.7

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy