Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
Alternate Names: St. Amand Clay, GSA
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 19.22% | 1.00 | |
| SiO2 | 66.30% | 5.85 | |
| TiO2 | 0.86% | 0.06 | |
| Fe2O3 | 1.41% | 0.05 | |
| CaO | 0.22% | 0.02 | |
| MgO | 0.15% | 0.02 | |
| K2O | 1.68% | 0.09 | |
| Na2O | 0.32% | 0.03 | |
| MnO | 0.02% | - | |
| LOI | 8.27% | n/a | |
| Oxide Weight | 478.58 | ||
| Formula Weight | 521.73 | ||
Dug in St. Amand France buy local potters for their own consumption, but Solargil (belongs to the WBB group) is digging it and retailing it as stoneware clay with the commercial name GSA .
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| Drying Shrinkage | 4.8% at 19% H2O |
|---|---|
| Firing Shrinkage | 11% total shrinkage at 1280°C |
| Water absorption | 0.2% water absorption (fired at 1280°C) |